The chemical composition of G-X6CrNiMo1810 steel grade typically includes:
– Carbon (C): 0.08%
– Silicon (Si): 1.00%
– Manganese (Mn): 2.00%
– Phosphorus (P): 0.04%
– Sulfur (S): 0.03%
– Chromium (Cr): 16.50%
– Nickel (Ni): 10.00%
– Molybdenum (Mo): 2.00%
The mechanical properties of G-X6CrNiMo1810 steel grade are as follows:
– Tensile strength: 550 MPa
– Yield strength: 240 MPa
– Elongation at break: 60%
– Modulus of elasticity: 200 GPa
– Hardness: 210 HB
The technical properties of G-X6CrNiMo1810 steel grade include its ability to withstand high temperatures and corrosion resistance. It is known for its excellent weldability, making it suitable for construction applications. This steel grade also has good thermal and electrical conductivity.
G-X6CrNiMo1810 steel grade is considered an eco-friendly alternative for sustainable construction due to its recyclability. It can be easily recycled and reused, reducing the environmental impact associated with new material production. Additionally, its corrosion resistance properties minimize maintenance and replacement needs, further contributing to sustainability in construction projects.