仕様:
The Future of X6CrNiTi1811 Steel Grade: Trends and Innovations
機械的性質:
– Tensile strength: 500-700 MPa
– Yield strength: 200-350 MPa
– Elongation: 40-60%
– Hardness: 150-250 HB
技術的特性:
– 密度: 7.9 g/cm3
– Melting point: 1400-1450°C
– Thermal conductivity: 15-20 W/m·K
– Electrical resistivity: 0.75-0.80 μΩ·m
化学組成:
– 炭素(C):最大0.08%
– シリコン (Si): 最大 1.00%
– Manganese (Mn): 2.00% max
– リン(P):最大0.045%
– 硫黄(S):最大0.03%
– Chromium (Cr): 16.00-18.00%
– Nickel (Ni): 10.00-14.00%
– Titanium (Ti): 1.50-3.00%